Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra DS16 - PA1010 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra DS16:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid Terra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明

Medium-viscosity polyamide 1010

VESTAMID® Terra DS16 NC is a medium-viscosity PA 1010 basic polymer. VESTAMID® Terra DS16 is semi-crystalline, which is the reason for its high mechanical resistance and chemical stability. It absorbs only little water. As a result its mechanical properties vary little when exposed to changing environmental humidity, and the material features a high dimensional stability.
 
VESTAMID® Terra DS16 can be used to manufacture films with good transparency.

The high melting point of VESTAMID Terra DS16 compounds results in a high heat deflection temperature that can be advantageous for some applications.
 
VESTAMID® Terra DS16 occupies a position between the high-performance long-chain polyamides such as PA 12 and PA 1212 and the standard polyamides PA 6 and PA 66, which have a shorter chain length.

VESTAMID® Terra DS16 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
 
VESTAMID® Terra is a group of new poly­amides, the monomers for which are based entirely or partly on renewable raw materials.

VESTAMID® Terra DS is the polycondensation product of 1,10-decamethylene diamine (D) and 1,10-dodecanedioic acid (sebacic acid-S). Because both monomers are extracted from castor oil, VESTAMID® Terra DS is based on natural, bio-based and renewable resources up to 100%.

The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM

加工/物理特性干 / 已调节单位Test Standard
ISO数据
模塑收缩率, 平行 1.4 / * % ISO 294-4, 2577
模塑收缩率, 垂直 1.5 / * % ISO 294-4, 2577
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 1700 / 1250 MPa ISO 527
屈服应力 54 / 48 MPa ISO 527
屈服伸长率 5 / 22 % ISO 527
名义断裂伸长率 >50 / >50 % ISO 527
无缺口简支梁冲击强度, +23°C N / N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C N / N kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 7 / 7 kJ/m² ISO 179/1eA
Type of failure C / C - -
简支梁缺口冲击强度, -30°C 7 / 5 kJ/m² ISO 179/1eA
Type of failure C / C - -
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 200 / * °C ISO 11357-1/-3
玻璃化转变温度, 10°C/min 37 / * °C ISO 11357-1/-2
热变形温度, 1.80 MPa 55 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 136 / * °C ISO 75-1/-2
维卡软化温度, B 171 / * °C ISO 306
线性热膨胀系数, 平行 115 / * E-6/K ISO 11359-1/-2
线性热膨胀系数, 垂直 135 / * E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
测试用试样的厚度 1.6 / * mm -
电性能干 / 已调节单位Test Standard
ISO数据
相对介电常数., 100Hz 3.6 / - - IEC 62631-2-1
相对介电常数., 1MHz 3.1 / - - IEC 62631-2-1
体积电阻率 >1E13 / 8.3E11 Ohm*m IEC 62631-3-1
介电强度 37 / - kV/mm IEC 60243-1
其它性能干 / 已调节单位Test Standard
吸水性 1.8 / * % 类似ISO 62
吸湿性 1.4 / * % 类似ISO 62
密度 1040 / - kg/m³ ISO 1183
典型数据
加工方法
注塑, 薄膜挤出成型, 其它挤出成型
供货形式
粒料, 碎粒料
特殊性能
经热稳处理的/耐热的, 透明.
耐化学试剂
通用耐化学性
Certifications
生物相容
地区供应
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com